Device parameters for perovskite solar cells with spin-coated and RFRS TiO2 ETL after annealing for 1 h at 450 °C.
Devices | PCE (%) | FF (%) | ||
---|---|---|---|---|
Spin-coated TiO2 | 16.044 | 1.017 | 21.625 | 72.902 |
RFRS TiO2 | 16.463 | 1.028 | 21.555 | 74.269 |