Fig. 4. Top-view SEM images of MoS2 with the precursor concentration and spin-coating speed of (a) 0.024 M and 2,000 rpm (solvent: DMF only) with the white circles indicating the features formed due to agglomeration of the precursor and (b) 0.012 M and 2,000 rpm (solvent: DMF only).